Grade :
|
X3CrNiCu18-9-4建筑用耐腐蝕鋼棒材
|
|
|
|
|
|
|
|
Number:
|
1.4567
|
|
|
|
|
|
|
|
Classification:
|
奧氏體不銹鋼
|
|
|
|
|
|
|
|
Density:
|
7.9 g/cm 3
|
|
|
|
|
|
|
|
Standard:
|
|
|
|
|
|
|
|
|
EN 10088-3:2005不銹鋼。一般用途耐腐蝕鋼的半成品、棒材、線材、型材和光亮產品的交貨技術條件
|
|
|
|
|
|
|
|
EN 10269:1999具有規定高溫和/或低溫性能的緊固件用鋼和鎳合金
|
|
|
|
|
|
|
|
EN 10263-5:2001冷鐓和冷擠壓用鋼條、棒材和線材。不銹鋼交貨技術條件
|
|
|
|
|
|
|
|
EN 10088-1:2005不銹鋼。不銹鋼清單
|
|
|
|
|
|
|
|
EN 10088-5:2009不銹鋼。建筑用耐腐蝕鋼棒材、棒材、線材、型材和光亮產品的交貨技術條件
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Equivalent grades:
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Chemical composition % of steel X3CrNiCu18-9-4 (1.4567): EN 10088-3-2005
|
|
|
|
|
|
|
|
|
C
|
Si
|
Mn
|
Ni
|
P
|
S
|
Cr
|
N
|
Cu
|
max 0.04
|
max 1
|
max 2
|
8.5 - 10.5
|
max 0.045
|
max 0.03
|
17 - 19
|
max 0.11
|
3月4日
|
|
|
|
|
|
|
|
|
|
Mechanical properties of steel X3CrNiCu18-9-4 (1.4567)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Rm - Tensile strength (MPa) (+A)
|
450-650
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Rm - Tensile strength (MPa) (+AT+C)
|
700-740
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Rp0.2 0.2% proof strength (MPa) (+A)
|
175
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
A - Min. elongation at fracture (%) (+A)
|
45
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Nominal diameter (mm):
|
2 - 50
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Z - Reduction in cross section on fracture (%)
|
63-68
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Brinell hardness (HB): (+A)
|
215
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|